Please use this identifier to cite or link to this item:
http://idr.nitk.ac.in/jspui/handle/123456789/10317
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Srinivasan, K. | - |
dc.contributor.author | Venugopal, P. | - |
dc.date.accessioned | 2020-03-31T08:18:55Z | - |
dc.date.available | 2020-03-31T08:18:55Z | - |
dc.date.issued | 2008 | - |
dc.identifier.citation | Materials and Manufacturing Processes, 2008, Vol.23, 4, pp.342-346 | en_US |
dc.identifier.uri | http://idr.nitk.ac.in/jspui/handle/123456789/10317 | - |
dc.description.abstract | Compression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India. | en_US |
dc.title | Compression testing of Ti-6Al-4V in the temperature range of 303-873 K | en_US |