Please use this identifier to cite or link to this item: http://idr.nitk.ac.in/jspui/handle/123456789/11017
Full metadata record
DC FieldValueLanguage
dc.contributor.authorSomasundaram, B.
dc.contributor.authorJegadeeswaran, N.
dc.contributor.authorMadhu, G.
dc.contributor.authorRamesh, M.R.
dc.date.accessioned2020-03-31T08:30:44Z-
dc.date.available2020-03-31T08:30:44Z-
dc.date.issued2017
dc.identifier.citationInternational Journal of Mechanical Engineering and Technology, 2017, Vol.8, 8, pp.1124-1134en_US
dc.identifier.urihttp://idr.nitk.ac.in/jspui/handle/123456789/11017-
dc.description.abstractIn the present study, (Cr3C2-35%NiCr) +5%Si cermet coatings were deposited on a Fe based T22 steel substrate to reduce the damage caused by erosion boiler applications. Erosion studies were conducted on uncoated as well as HVOF coated steels. The erosion experiments were carried out using an air-jet erosion test rig according to ASTM G-76 standard at a velocity of 30 m/s and at different impingement angles of 30 , 60 and 90 . Silica sand particles of size ranging between 150 to180 ?m were used as erodent. Analysis of weight-loss data and volumetric steady state erosion rates for different coatings and substrate alloys are evaluated. The bare T22 steel followed ductile erosion mode where as (Cr3C2-35%NiCr) +5%Si coating exhibited mixed behaviour respectively.en_US
dc.titleErosion behaviour of HVOF sprayed (CR3C2-35%NICR) +5%Si coatingsen_US
dc.typeArticleen_US
Appears in Collections:1. Journal Articles

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.