Please use this identifier to cite or link to this item: http://idr.nitk.ac.in/jspui/handle/123456789/16175
Full metadata record
DC FieldValueLanguage
dc.contributor.authorShajahan I.
dc.contributor.authorDasari H.P.
dc.contributor.authorSaidutta M.B.
dc.date.accessioned2021-05-05T10:29:54Z-
dc.date.available2021-05-05T10:29:54Z-
dc.date.issued2020
dc.identifier.citationInternational Journal of Hydrogen Energy Vol. 45 , 48 , p. 25935 - 25944en_US
dc.identifier.urihttps://doi.org/10.1016/j.ijhydene.2020.06.163
dc.identifier.urihttp://idr.nitk.ac.in/jspui/handle/123456789/16175-
dc.description.abstractThe present study investigates the effect of sintering additives (Li, Co, Fe, and Mg) on the sintering kinetic behavior of the praseodymium-doped-ceria (PDC) electrolyte of solid oxide electrolyzer cell. 3Li-PDC, 3Co-PDC, 3Fe-PDC, and 3 Mg-PDC pellets were obtained from the synthesis of PDC nano-powder by microwave-assisted co-precipitation method using isopropyl alcohol as a solvent and followed by sintering additive wetness impregnation method. Linear shrinkage and shrinkage rate data suggest a positive sintering effect for 3Li-PDC and 3Co-PDC pellets and a negative sintering effect for 3 Mg-PDC and 3Fe-PDC pellets than compared to PDC pellets alone. The addition of lithium as a sintering additive (3Li-PDC) had reduced the sintering temperature of PDC from 1100 °C to 850 °C. For PDC, 3Li-PDC, 3Co-PDC, 3Fe-PDC and 3 Mg-PDC pellets sintered at 1100 °C, 850 °C, 1000 °C, 1200 °C, 1100 °C for 2 h resulted in a relative density of 93.6 ± 0.25, 95.8 ± 0.45, 95.0 ± 0.20, 92.7 ± 0.10, and 94.5 ± 0.10%, respectively. The XRD patterns of the sintered PDC pellets suggested a secondary phase formation (PrO2) in 3Co-PDC, 3Fe-PDC, and 3 Mg-PDC pellets indicating that the addition of these sintering aids results in poor solubility limit of Pr in CeO2. On the other hand, XRD patterns of PDC and Li-PDC sintered pellets displayed no secondary peak indicating good solid-solution formation. The activation energy of the 3Li-PDC pellet is obtained from CHR and Dorn methods and was found to be 182 kJ/mol and 196 kJ/mol. From the CHR method, for the 3Li-PDC pellet, the initial sintering behavior is by the grain boundary diffusion mechanism (m = ~2). © 2020 Hydrogen Energy Publications LLCen_US
dc.titleEffect of sintering aids on sintering kinetic behavior of praseodymium doped ceria based electrolyte material for solid oxide cellsen_US
dc.typeArticleen_US
Appears in Collections:1. Journal Articles

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.